7/5/2005

I finished drilling and deburring the rear spar components. I then acid etched and Alodined all of the parts, dried them with an air hose and then primed them. The temperature was above 100 degrees and the humidity was really high. You are supposed to leave the Alodine on for 2 minutes but it kept drying.

 

email: Luis Luciani 

7.5 hours